Decision Context and Winning Criteria
Agriculture chair mold selection hinges on durability under field stress and production cost. PC excels in impact resistance and dimensional stability—critical for outdoor seating exposed to UV and mechanical shock—but demands 280–320°C processing and tighter gate design. PE reduces material spend and flows more readily at lower pressures, yet sacrifices the optical clarity and long-term stiffness (PC's 2.3 GPa flexural modulus) that extend chair service life. Choose PC when chairs require transparent components, high-impact zones, or multi-year outdoor durability. Select PE when cost-per-unit dominates and opaque, lower-strength seating meets specification. Injection pressure for PC runs 800–1600 bar; wall thickness typically 1.5–4 mm to balance cooling and structural load.